ASTM A 312—09 Standard Specification for Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes (PDF Download)
The PDF/Redline Download option contains PDF files of both the I-Code and a Redline version of the I-Code which shows changes from the previous edition marked in the color red. With the Redline you can see what has been changed from the previous edition. This option is a searchable PDF download that requires a PDF Reader. It is mobile compatible with mobile tablets and smart phones that support the PDF format. The PDF Download is licensed per individual, who may place the file on up to four electronic devices for their personal use. Distribution of the PDF is not permitted. For a volume license the PDF is licensed to the person to which it is assigned. Use on a local area network or other network is not permitted.
This guide covers standard specification for seamless, straight-seam welded, and cold worked welded austenitic stainless steel pipe intended for high-temperature and general corrosive service. Several grades of steel shall conform to the required chemical composition for carbon, manganese, phosphorus, sulfur, silicon, chromium, nickel, molybdenum, titanium, columbium, tantalum, nitrogen, vanadium, copper, cerium, boron, aluminum, and others. All pipes shall be furnished in the heat-treated condition in accordance with the required heat treating temperature and cooling/testing requirements. Tensile properties of the material shall conform to the prescribed tensile strength and yield strength. The steel pipe shall undergo mechanical tests such as transverse or longitudinal tension test and flattening test. Grain size determination and weld decay tests shall be performed. Each pipe shall also be subjected to the nondestructive electric test or the hydrostatic test.
This standard is referenced in the 2012 International Swimming Pool and Spa Code™.
| Description: | This guide covers standard specification for seamless, straight-seam welded, and cold worked welded austenitic stainless steel pipe intended for high-temperature and general corrosive service. Several grades of steel shall conform to the required chemical composition for carbon, manganese, phosphorus, sulfur, silicon, chromium, nickel, molybdenum, titanium, columbium, tantalum, nitrogen, vanadium, copper, cerium, boron, aluminum, and others. All pipes shall be furnished in the heat-treated condition in accordance with the required heat treating temperature and cooling/testing requirements. Tensile properties of the material shall conform to the prescribed tensile strength and yield strength. The steel pipe shall undergo mechanical tests such as transverse or longitudinal tension test and flattening test. Grain size determination and weld decay tests shall be performed. Each pipe shall also be subjected to the nondestructive electric test or the hydrostatic test. This standard is referenced in the 2012 International Swimming Pool and Spa Code™. |
|---|---|
| Pages | 12 |
| Code Year | 2012 |
| Publisher | ASTM International |
| Language | English |