This is a demo store. No orders will be fulfilled.
ASTM C 920—08 Standard for Specification for Elastomeric Joint Sealants (PDF Download)
The PDF/Redline Download option contains PDF files of both the I-Code and a Redline version of the I-Code which shows changes from the previous edition marked in the color red. With the Redline you can see what has been changed from the previous edition. This option is a searchable PDF download that requires a PDF Reader. It is mobile compatible with mobile tablets and smart phones that support the PDF format. The PDF Download is licensed per individual, who may place the file on up to four electronic devices for their personal use. Distribution of the PDF is not permitted. For a volume license the PDF is licensed to the person to which it is assigned. Use on a local area network or other network is not permitted.
This specification covers the properties of a cured single- or multicomponent cold-applied elastomeric joint sealant for sealing, caulking, or glazing operations on buildings, plazas, and decks for vehicular or pedestrian use, and types of construction other than highway and airfield pavements and bridges. A sealant qualifying under this specification shall be classified as to type, grade, class and use as follows: type S - a single-component sealant, type M - a multicomponent sealant, grade P - a pourable or selfleveling sealant, grade NS - a nonsag or gunnable sealant, class 100/50, class 50, class 35, class 25, class 12.5, use T, use NT, use I, use M, use G, use A, and use O. A single-component sealant shall be a uniform mixture of a consistency suitable for immediate application by hand or pressure caulking gun or by hand tool. A multicomponent chemically curing sealant shall be furnished in two or more components. A single-component and multicomponent sealant, when stored in the original unopened container at temperatures of not more than 27°C (80°F) shall be capable of meeting the requirements for at least 6 months after date of delivery. Grade P (pourable or selfleveling) sealant shall have the required flow characteristics, it shall exhibit a smooth, level surface. Grade NS or gunnable sealant shall have the required flow characteristics such that when tested in vertical displacement. Type S, grade P, and grade NS sealant shall not be less than the given extrusion rate when tested. Type M and grade P sealant, when tested shall be not less than the given extrudable rate 3 h after mixing. Use T (traffic) sealant shall have a hardness reading, after being properly cured, of not less than 25 or more than 50 when tested. Use NT (nontraffic) sealant shall have a hardness reading, after being properly cured, of not less than 15 or more than 50 when tested. The sealant shall not lose more than 7 % of its original weight or show any cracking or chalking when tested. There shall be no transfer of the sealant to the polyethylene film when tested at 72 h. The sealant shall not cause any visible stain on the top surface of a white cement mortar base when tested. The adhesion and cohesion after cyclic movement shall be tested to meet the requirements prescribed. The adhesion-in-peel test shall be performed to meet the requirements precribed. The adhesion-in-peel after ultraviolet exposure through glass shall be determined to meet the requirements prescribed. The accelerated weathering effects, and sealants exposed to continuous immersion shall be determined to meet the requirements prescribed.
This standard is referenced in the 2012 International Building Code® and the International Residential Code®.
| Description: | This specification covers the properties of a cured single- or multicomponent cold-applied elastomeric joint sealant for sealing, caulking, or glazing operations on buildings, plazas, and decks for vehicular or pedestrian use, and types of construction other than highway and airfield pavements and bridges. A sealant qualifying under this specification shall be classified as to type, grade, class and use as follows: type S - a single-component sealant, type M - a multicomponent sealant, grade P - a pourable or selfleveling sealant, grade NS - a nonsag or gunnable sealant, class 100/50, class 50, class 35, class 25, class 12.5, use T, use NT, use I, use M, use G, use A, and use O. A single-component sealant shall be a uniform mixture of a consistency suitable for immediate application by hand or pressure caulking gun or by hand tool. A multicomponent chemically curing sealant shall be furnished in two or more components. A single-component and multicomponent sealant, when stored in the original unopened container at temperatures of not more than 27°C (80°F) shall be capable of meeting the requirements for at least 6 months after date of delivery. Grade P (pourable or selfleveling) sealant shall have the required flow characteristics, it shall exhibit a smooth, level surface. Grade NS or gunnable sealant shall have the required flow characteristics such that when tested in vertical displacement. Type S, grade P, and grade NS sealant shall not be less than the given extrusion rate when tested. Type M and grade P sealant, when tested shall be not less than the given extrudable rate 3 h after mixing. Use T (traffic) sealant shall have a hardness reading, after being properly cured, of not less than 25 or more than 50 when tested. Use NT (nontraffic) sealant shall have a hardness reading, after being properly cured, of not less than 15 or more than 50 when tested. The sealant shall not lose more than 7 % of its original weight or show any cracking or chalking when tested. There shall be no transfer of the sealant to the polyethylene film when tested at 72 h. The sealant shall not cause any visible stain on the top surface of a white cement mortar base when tested. The adhesion and cohesion after cyclic movement shall be tested to meet the requirements prescribed. The adhesion-in-peel test shall be performed to meet the requirements precribed. The adhesion-in-peel after ultraviolet exposure through glass shall be determined to meet the requirements prescribed. The accelerated weathering effects, and sealants exposed to continuous immersion shall be determined to meet the requirements prescribed. This standard is referenced in the 2012 International Building Code® and the International Residential Code®. |
|---|---|
| Pages | 4 |
| Code Year | 2012 |
| Publisher | ASTM International |
| Language | English |